彩钢净化板板材发软、产生色差的原因

来源:http://www.jnhscg.com 日期:2022-12-29

目前,市场上做彩钢净化板的厂家也是越来越多,各种质量问题也随之而来。下面济南彩钢夹芯板厂来讲讲彩钢净化板板材发软、产生色差的原因!

At present, there are more and more manufacturers making color steel purification plates in the market, and various quality problems follow. Next, Jinan Color Steel Sandwich Panel Factory will talk about the reasons for the softening and color difference of color steel purification plate!

彩钢净化板发软的缘由:

Reasons for softening of color steel purification plate:

1、凝胶时间过长。

1. The gel time is too long.

2、净化板色块的树脂不含蜡。

2. The resin of the color block of the purification plate does not contain wax.

3、铸造时温度过高或过低。

3. The temperature is too high or too low during casting.

4、洁净室环境温度过高。

4. The ambient temperature of the clean room is too high.

彩钢净化板产生色差的缘由:

Reasons for color difference of color steel purification plate:

1、树脂混合物搅拌不充沛。

1. The resin mixture is not stirred sufficiently.

2、颜料丈量错误。

2. Paint measurement error.

3、不运用预混分散搅拌。

3. Do not use premixed dispersion mixing.

4、烘房局部过热,板材受热不均。

4. The drying room is partially overheated and the plates are unevenly heated.

20211124105083.jpg

此外在工厂彩钢净化板预制时,根据经验,充分考虑门洞、窗洞和接缝之间的间隙和安装余量。在整个运输和安装过程中,防止划痕、重压和表面碰撞,防止凹坑和划痕无法纠正。

In addition, during the prefabrication of color steel purification plates in the factory, the gap and installation allowance between door openings, window openings and joints shall be fully considered according to experience. During the whole process of transportation and installation, prevent scratches, heavy pressure and surface collision, and prevent pits and scratches from being uncorrectable.

熟悉图纸,仔细审查彩钢净化板的平面布置、节点要求、彩钢净化板与建筑的关系、彩钢净化板本身的颜色、填充物和基本尺寸要求、门窗的尺寸和布局,彩钢净化板隔断中辅助材料的类型等未知内容。

Get familiar with the drawings, carefully review the unknown contents such as the plane layout, node requirements, the relationship between the color steel purification plate and the building, the color of the color steel purification plate itself, filler and basic size requirements, the size and layout of doors and windows, and the type of auxiliary materials in the color steel purification plate partition.

密封硅胶应安装在彩板上,卫生条件良好。清洁和除尘后,应进行统一。否则,硅胶接缝容易被污染和发黑。硅胶打浆后24小时内,不应有大量灰尘作业和用水冲洗地面,这可能会影响密封硅胶的固化和牢固性。

The sealing silica gel shall be installed on the color plate in good sanitary condition. After cleaning and dedusting, it shall be unified. Otherwise, the silicone joint is easy to be polluted and blackened. Within 24 hours after the silica gel is grouted, there should not be a lot of dust operations and the ground should not be washed with water, which may affect the curing and firmness of the sealing silica gel.

其实想要保证板材的颜色不受影响,需要大家对整个生产过程进行把控,特别是在刷涂外层涂料时,不仅要注意涂抹均匀,而且涂料也要符合使用要求才可以。更多相关内容就来我们网站http://www.jnhscg.com咨询吧!

In fact, to ensure that the color of the board is not affected, we need to control the entire production process, especially when brushing the outer layer of paint, we should not only pay attention to the uniform application, but also the paint should meet the use requirements. More relevant content will come to our website http://www.jnhscg.com Consult!